Customization: | Available |
---|---|
Feature: | Corrosion Resistance, High-Thermal Conductivity, Thermal Shock Resistance |
Manufacturing Technique: | Compression Moulding |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Density g/cm³ | 1.75-1.9 |
Resistivity μΩ·m | ≤12 |
Compressive strength Mpa | ≥70 |
Porosity % | ≤26 |
Elasticity Modulus Gpa | 6-18 |
Thermal expansion coefficient 10-6/ºC | 1.47-4.25 |
Ash content % | ≤0.05 |
Temperature resistance ºC | ≤4350ºC |
Item | Unit | 2.0mm HNLT |
2.0mm HNLT |
Bluk Density | g/cm3 | ≯12 | ≯9 |
Electric Resitivity | μΩm | ≮1.58 | ≮1.70 |
Compressive Strength | Mpa | ≮19 | ≮30 |
Bending Strength | Mpa | ≮7.8 | ≮13 |
Ash Content | % | ≯0.3 | ≯0.3 |
C.T.E | 10-6/ºC | ≯2.0 | ≯2.2 |
Bulk Density g/cm³ | 1.9-2.1 |
Porosity % | 10-14 |
Carbon Content % | 30-45 |
Silicon Carbide content % | ≥48 |
Temperature resistance ºC | 1665 |